Small Member Group: Members Posts: 1,697 Joined: 30-April 03 From: Colorado Member No.: 633 |
Built a muffler last night (really pleased with how it came out and sounds). Woke up with a sore throat. By lunch a had just a touch of the shakes. Called the FLAPS where I bought some of the piping and they guy said it was galvanised. When I bought the stuff, I specifically asked about this, as it was hard to tell if the parts were coated (not the usual sheen). The other guy said he thought they were just aluminized and would be fine to weld. Being a beginner - I believed him.
Any idea how this will last? I spent a continuous 2-3 hours last night breathing this crap. I litterally feel like I have a mild flu. (IMG:style_emoticons/default/headbang.gif) |
charliew |
Jul 30 2010, 05:03 PM
Post
#2
|
Advanced Member Group: Members Posts: 2,363 Joined: 31-July 07 From: Crawford, TX. Member No.: 7,958 |
I'm sorry but I never had a good experience trying to weld through galvanize with a mig. I have welded it pretty trouble free on angle that was gal though with a stick welder. I'm sure it was the flux on the rod.
|