surfbus66
Oct 1 2010, 10:34 AM
I'm ready to put the jugs back on motor after cleaning and inspection. I know the factory didn't use any sealant, but should I now? (High Temp RTV)?
surfbus66
Oct 2 2010, 05:44 AM
QUOTE(nathansnathan @ Oct 1 2010, 09:31 AM)
hylomar or permatex 3h
Thanks. I'm assuming I put a thin coating on both sides of sealing ring?
Cevan
Oct 2 2010, 06:26 AM
I used Curil T. By sealing ring, I assume you mean the shim? I put the Curil T on both sides of the shim and on the jug. No issues to date.
Drums66
Oct 2 2010, 11:32 AM
.....Very minimal, if any?